www.durafix.com

Discuss!


p.s. I barely got half way through the vid and I skipped ahead to eBay and bought a pack of 20!

p.p.s. if anyone is concerned about strength, there's another video when a guy has welded 10mm plates of ally together at right angles, smacks one side with a hammer and the ally begins to bend before the weld fails!

p.p.p.s. http://cgi.ebay.com.au/ws/eBayISAPI.dll?ViewItem&item=270768970566&ssPageName=STRK:MEWNX:IT#ht_3105wt_1139
Link to comment
https://www.sau.com.au/forums/topic/368666-durafix-easy-weld/
Share on other sites

Looks handy to have around, but its around $50 for 40 rods and you need an oxy.

i'd love to try it for rim repairs though

See that eBay link? $11 US for approx 10 rods... Looks like one does a fair bit too...

You don't need an oxy set-up, just a butane torch...

Pretty fkn awsome if it holds up as well as it looks...

Ha ha... I wanna see someone 'solder' up a cooler pipe work set up-

I've bought some for the sole purpose to re-doing my intercooler piping and making an airbox, so I'll update in this thread how I go!

Edited by StealthX

this stuff has been around for yrs i saw a display at a car show over 20 yrs ago i was pretty impressed then . ive never used it but i can see it would be handy to have a few rods in the workshop.

  • 3 months later...

I used this stuff to make up an intake for my car. Turned out OK, considering I have no experience with welding etc.

I used a LPG gas bottle from my bar-b-q, with an appropiate nozzle, to heat up the material. One thing to remember, if you are making something with a few separate parts (like I did), when you heat it up again to stick the new bit on, there's a big chance the original "weld" will start to run. To help with this problem I bought a block of modelling clay and pushed some around the first bit/s to act like a heat sink.

post-76144-0-30043900-1318242557_thumb.jpg

  • 2 weeks later...

anyone know if they have something similar for steel?

i've got a stick welder and we're trying to modify a pocket bike exhaust onto a motorised push bike (using the band expander)

the cheap chinese steel is so thin that its got a few holes in it

just want something solder like that will work like this does

  • 2 weeks later...

They usually have a stand at farm machinery days and will weld up any alloy part you bring in to get done. They are very good at it and make it look very easy. I've tried it in different things and it works OK, but I found that using the normal commercially available alloy brazing flux and 10% mag rods is about the same. This was using a Dillon/Henrob oxy.

anyone know if they have something similar for steel?

i've got a stick welder and we're trying to modify a pocket bike exhaust onto a motorised push bike (using the band expander)

the cheap chinese steel is so thin that its got a few holes in it

just want something solder like that will work like this does

Chinese metal for things like your talking about is usually terrible stuff to play with. Its usually recycled tseel with inclusions all through it. And then you say it is an exhaust pipe or some such - double whammy. Nothing like exhaust pipe for dirt and crap in the metal.

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now


  • Similar Content

  • Latest Posts

    • The correct answer is body colour. Admittedly it does look pretty handsome as-is in grey.
    • I'm surprised there isn't any interest in this.
    • Por qué no los dos? Body colour red with black stripes down centre, onto bonnet and bootlid.
    • From my bolts, standard M8 with 1.25mm thread pitch (M8x1.25mm).    Length is 19mm under the head and has a captive 18mm OD flat washer.   20mm length from a bolt shop is what you'll be able to get.   Make sure they're zinc plated.    If you're concerned about strength, grade 8.8 will be more than enough. Original PN is 01121-04971.  Now discontinued according to Amayama but that's because it's one of the parts that's been captured by the Heritage program, which explains the ridiculous price.   New PN is 01121-RHR20: https://nismodirect.com/nismo-heritage-bolt-pin-hinge-hood-bnr32-nissan-skyline-gt-r-01121-rhr20-01121-04971/ About AUD33 converted from Yen in the above link but that's just one example. Interesting that the hinge-to-body bolts are still available non-heritage.....PN 08116-8161G around $2 each (amayama).    Same thread but 16mm long.
    • Well, if that filter was impeding fluid flow, then it could have similar effects to faulty solenoids. The TCU will register a fault when it does something (ie, changes the state of a solenoid) and does not detect the required result. If there are other causes that can make the same lack of result, then they will be indistinguishable to the expected cause for which the TCU has a code.
×
×
  • Create New...