Review: Mothers NuLens™ Headlight Renewal Kit

European cars seem to struggle with maintaining high levels of headlight condition.

While Japanese cars seem to suffer from fading/clouding, Euro's get pitting and a rough coating over them. We have 2 European cars and they've both fallen victim to this pitting and coating. 

I bought the Mothers NuLens™ Headlight Renewal Kit to try to clean up the headlights on my wife's 2007 Volkswagen Passat.

07251_Mothers_NuLens_DIY_Headlight_Restoration_Kit.jpg

Here's some pics of the headlight before I started. You can see just how bad the pitting and scratches are.

20161223_173556.jpg

20161223_173603.jpg

20161223_173611.jpg

 

So, the process is very simple;

  1. tape up your paintwork
  2. I put a hose on very low just dribbling over the headlight to keep it wet.
  3. Sand with the supplied 800 grit pad (you'll see in the below pics I needed to do this longer)
  4. When you have a uniform haze and it feels smooth, sand with the 1500 grit pad
  5. When the haze is uniform again, dry the light and 
  6. Sand with the 3000 grit foam pad.
  7. Lastly, use the Powerball and polish to polish the headlight.

So, after about 20 mins, the result is amazing. You can see that some scratches still exist, I can't feel these so I missed them on the 800 grit stage. I'm planning on redoing the sanding next week to see if I can improve it. But, even without doing that again, it looks (and feels) incredible.

20161223_180408.jpg

20161223_180404.jpg

 

I would recommend this kit to anybody who has external defects on their headlights. (A lot of R33's get hazing/clouding on the inside of the headlight.)

This is a 5 star product for sure. $40 very well spent.

 

  • Like 3

All these products are great but without some kind of UV protection the problem will be back, and faster than before, since all the sanding and polishing has now left bare plastic with zero protection

there are a couple of kits with spray on clear coat, i'm testing one now

All these products are great but without some kind of UV protection the problem will be back, and faster than before, since all the sanding and polishing has now left bare plastic with zero protection
there are a couple of kits with spray on clear coat, i'm testing one now


So is the process the same with the addition of a clear coat spray once completed ? I'm looking into this myself as I have three cars that could do with similar attention
On 12/24/2016 at 2:10 PM, blade511 said:

 


So is the process the same with the addition of a clear coat spray once completed ? I'm looking into this myself as I have three cars that could do with similar attention

 

exactly the same process yeah. the clear coat is some special stuff that sticks to plastic without primer and has built in UV blocking ability

I've used that Glassy Lite kit worked well also Invision headlight kit has decent uv sealant. 

Another thing I've used is 303 aerospace protectant.

Best thing to do is just buy a bottle of UV sealant. if you can't get it locally, you can from the U.S then just sand/polish.

 

I bought a meguiars headlight polishing kit. It's just some sanding pads (various grades), and polish and the uv protectant.

Did the first headlight with it and it turned out ok for a lot of work. Then had to remove the headlights to change bulbs  (yes, really) so I attacked the other light. Started with a sanding block and 320 grade wet and dry. Then repeated with 800, 1500 and finished with 2000 grade. After that I hit it with the polisher working through 3 grades of polish and finished with some of the uv protectant from the kit.

the second light turned out heaps better - similar amount of  work but much easier just buying the right grades of sandpaper.  It helps if you have a ROP for polishing though.

It's worth getting a bottle of the uv protectant though. Everything else is just normal sanding/ polishing stuff.

  • Like 1

I've started coating my headlights weekly with the 303 protectant as it has UV protection.

@warps I did this last year with my Bora, just bought the sand paper grades and did it myself. The reason I grabbed the Mothers kit this time is because of the polish and the polish ball to really get them sparkling, which it does. I will just use the sand paper directly from now on.

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now


  • Similar Content

  • Latest Posts

    • Yes, but no. You need to keep the mating surfaces bare (ie the flat faces where the caliper and upright pads touch the dogbone) and also the internal threads will remain bare (unless there are no internal threads - do they use nuts on all the bolts?). So you can slow down obvious external corrosion, but not all of it. Anodising would be required to provide decent protection to the alloy, but I'm not actually sure if you should anodise something that is all about the strength. Anodising does reduce strength significantly. Like, up to 50% on some alloys for high thickness coating.
    • Thanks   does painting on aluminium work or stop them from corroding?
    • 'Sgot nothing to do with them being Japanese. The climate in the north of Japan has similarities to the UK - the cars are made in the knowledge that they have snow and salt, and they rot there. Cars made in the US rot like buggery in the US. British cars have always rotted regardless of the weather. They will rot indoors in a climate controlled bubble! The brackets are not unsafe yet, but they will get that way. They may well corrode where the bolt threads are in contact and the bolts could just jump out without warning.
    • So unsafe would you say now?   little bit of has come off, guess road salt is a nightmare for Japanese car. Mx5 here have a well known issue or rotting 
    • Dissimilar metal corrosion. Aluminium is less noble than steel/iron, and will corrode preferentially when in contact with it and a conductive solution (ie, wet road salt). Tends to suggest that those brackets should be made in steel for a shitty climate like the UK.
×
×
  • Create New...